Counter-Rotating Parallel Twin Screw Barrel
  • Counter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw Barrel

Counter-Rotating Parallel Twin Screw Barrel

Nanhaiya Counter-Rotating Parallel Twin Screw Barrel is specially developed for PVC, PE, and WPC extrusion lines. As a professional screw barrel manufacturer in China since 2014, Nanhaiya focuses on high-quality extrusion solutions with competitive prices and stable performance. Our parallel twin screw barrels offer excellent torque balance, high output efficiency, and long service life, making them the preferred choice for global customers seeking reliable and efficient extrusion equipment.

Nanhaiya counter-rotating parallel twin screw barrel features screws that rotate in opposite directions, producing strong inter-screw shear for enhanced compounding and kneading. It is ideal for processing sensitive materials that require low thermal stress. The barrel is manufactured from high-grade 38CrMoAlA with a nickel-based tungsten carbide alloy layer for superior wear resistance. Each unit is precision machined to ensure exact clearance, providing smooth rotation and consistent material flow. This design is particularly effective for PVC pipes,PVC profiles, WPC panels, and polymer blends that require uniform dispersion.

Product Parameter (Specification)

Material

38CrMoAlA

Heat Treatment Hardness

HB260-320

Nitriding Hardness

HV950-1000

Nitriding Depth

0.50-0.70mm

Nitriding Brittleness

≤grade 1

Roughness

Ra0.4

Screw Straightness

0.015mm

Chrome Plating Hardness

HV≥950HV

Chrome Thickness

0.05-0.10mm

Bimetal Hardness

HRC60-65

Bimetal Depth

2.0-3.0mm

Product Feature and Application

The co-rotating design allows both screws to rotate in the same direction, producing strong intermeshing and continuous conveying action. This ensures high throughput and uniform melting, making it ideal for compounding, pipe extrusion, and sheet production. The barrel is crafted from premium steel and lined with nickel-based tungsten carbide alloy to resist wear and corrosion. Each barrel is finely machined for precise clearance, ensuring smooth rotation, consistent pressure, and reduced mechanical vibration.

Counter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw Barrel

Production Details

Each Nanhaiya parallel twin screw barrel undergoes advanced CNC machining and precision grinding. The surface is mirror-finished to minimize friction and improve plastic flow. The screw flight is hardened by nitriding or bimetallic alloy coating for long-term stability.

Counter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw BarrelCounter-Rotating Parallel Twin Screw Barrel
Hot Tags: Counter-Rotating Parallel Twin Screw Barrel, Manufacturer, Supplier, Factory
Send Inquiry
Contact Info
Welcome to our website! For inquiries about our products or pricelist, please leave your email to us and we will be in touch within 24 hours.