Twin Screw Extruder

Nanhaiya Twin Screw Extruder provides superior mixing, plasticizing, and degassing performance, especially for PVC and high-filling formulations. Designed with high torque and precise synchronization, it delivers efficient extrusion for pipe, profile, granulation, and sheet production.

Nanhaiya Twin Screw Extruder provides superior mixing, plasticizing, and degassing performance, especially for PVC and high-filling formulations. Designed with high torque and precise synchronization, it delivers efficient extrusion for pipe, profile, granulation, and sheet production.

Features & Applications

Key Features

• High torque gearbox for strong processing capabilities

• Excellent mixing uniformity and material dispersion

• Optional conical or parallel screw structures

• Forced feeding for stable material output

• Perfect for PVC and engineering plastics

Main Applications

• PVC pipe and profile extrusion

• Granulation of filler-modified materials

• WPC board, panel, and sheet extrusion

• Recycling and compounding processes

Twin Screw ExtruderTwin Screw ExtruderTwin Screw ExtruderTwin Screw ExtruderTwin Screw ExtruderTwin Screw Extruder

Product Details

Screw Configuration: Co-rotating synchronization for excellent mixing & conveying efficiency

Gearbox: High-torque structure, extended bearing life, stable transmission under heavy load

Barrel Structure: Multi-zone heating/cooling, optional vacuum venting for moisture & volatile removal

Material Options: 38CrMoAlA nitrided steel / W6Mo5Cr4V2 / HIP powder steel for high wear resistance

Feeding System: Forced feeder suitable for PVC powder and high-filling formulations

Temperature Control: PID intelligent control with independent zone regulation

Electrical System: International brands optional (Siemens / ABB / Schneider)

Screw Type:

Conical → More torque for PVC pipe & profile

Parallel → Better uniformity for granulation & WPC

Output: High-capacity design with energy-saving motor and optimized screw profile

Twin Screw ExtruderTwin Screw ExtruderTwin Screw ExtruderTwin Screw ExtruderTwin Screw ExtruderTwin Screw Extruder

Recommended Models

Model

Type

Screw Diameter

Motor Power

Output

(kg/h)

Application Focus

SJSZ-45/90

Conical

Φ45/90

15–18.5 kW

100–180

Small profile

SJSZ-51/105

Conical

Φ51/105

18.5–22 kW

150–250

Profile, soft PVC

SJSZ-65/132

Conical

Φ65/132

37–45 kW

250–380

PVC pipe/profile

SJSZ-80/156

Conical

Φ80/156

55–75 kW

350–500

Medium pipe

SJSZ-92/188

Conical

Φ92/188

110–160 kW

600–900

Large pipe/extrusion

Send Inquiry
Contact Info
Welcome to our website! For inquiries about our products or pricelist, please leave your email to us and we will be in touch within 24 hours.
X
We use cookies to offer you a better browsing experience, analyze site traffic and personalize content. By using this site, you agree to our use of cookies. Privacy Policy
RejectAccept