Model:40/45/50/55/60/65/75/80/90/120/130/150
Single Screw Barrel for HDPE Pipe Extrusion is designed for HDPE pipe production with HDPE materials. Screw geometry, barrel configuration and surface treatment can be selected according to the resin, equipment specifications and production requirements.
  • Material:

    38CrMoALA
Rating: 5.0
(Rating Count: 1)

Application in Hdpe Pipe Production

Hdpe pipe production requires a screw and barrel configuration that suits the material and the complete extrusion line. The Single Screw Barrel for HDPE Pipe Extrusion is selected according to the HDPE grade, feeding method, equipment layout and required output. Material characteristics can vary between suppliers and formulations, so the final design should be confirmed using actual processing information.


Technical Specifications

Material
38CrMoALA
Heat Treatment Hardness
HB260-320
Nitriding Hardness
HV950-1000
Nitriding Depth
0.50-0.70mm
Nitriding Brittleness
≤grade 1
Roughness
Ra0.4
Screw Straightness
0.015mm/m
Chrome Plating Hardness
HV≥950HV

Chrome Thickness

0.05-0.10mm

Bimetal Hardness

HRC60-65
Bimetal Depth
2.0-3.0mm

Screw Geometry and Plasticizing Performance

The feeding section, compression section and metering section influence material conveying, melting and pressure stability. The HDPE pipe extruder screw barrel should be evaluated with reference to resin flow behavior, screw speed, heating zones and downstream equipment. Screw diameter, L/D ratio, channel depth and optional mixing features are determined by the required process, rather than selected from a generic specification.



Barrel Materials and Surface Treatment

Screw and barrel materials should be chosen according to processing temperature, pressure, additives and wear conditions. Nitrided steel can be considered for suitable standard applications. Where abrasive fillers, recycled content or demanding operating conditions are involved, bimetallic or other wear-resistant options may be assessed. The correct solution depends on the actual formulation and expected service conditions.


Precision Manufacturing and Quality Inspection

Manufacturing may include material preparation, rough machining, heat treatment, precision machining, flight finishing and surface treatment. Inspection items can include screw diameter, flight profile, barrel bore, straightness, concentricity, matching clearance and surface condition. Each Single Screw Barrel for HDPE Pipe Extrusion should be produced against an approved drawing and checked according to the agreed technical requirements before delivery.



Customization and Equipment Matching

Extruders differ in screw diameter, L/D ratio, drive power, heating arrangement, connection dimensions and output range. Nanhaiya can review machine drawings, samples or existing component dimensions to discuss a replacement or customized design. The Single Screw Barrel for HDPE Pipe Extrusion must match the machine interface and the intended process. Special structures, venting sections or mixing elements should be confirmed before production.


Information for Technical Evaluation

For a quotation or design review, please provide the pipe diameter range, resin grade, target output and line speed, together with the extruder model, screw dimensions and current operating conditions. Photos of the existing screw and barrel, drawings and details of any processing problems are also useful. This information helps assess the Single Screw Barrel for HDPE Pipe Extrusion for the actual application and reduces uncertainty when confirming dimensions and configuration.







Send Inquiry
Contact Info
Welcome to our website! For inquiries about our products or pricelist, please leave your email to us and we will be in touch within 24 hours.
Rating:
5.0
X
We use cookies to offer you a better browsing experience, analyze site traffic and personalize content. By using this site, you agree to our use of cookies. Privacy Policy
RejectAccept